Wätsilä paraffin cooling cooler welding

1. welding process difficulties are as follows

Inner tank sealing

The liner is made of 304 stainless steel, 4mm thick. The six sides of the inner container and the pipe joint are fully welded to ensure the pressure-resistant sealing inside the inner container. The inner container shall be subjected to pressure test before leaving the factory, with a pressure of 3kg. Finned tube joints are made of 316 stainless steel, and 304 and 15800.00g kinds of stainless steel are welded. The welding process needs to be optimized to ensure good fusion and sealing.

Cleaning after welding in pipe

The welding of the pipe joint will cause pollution to the inner wall. The finned pipe is placed in the inner container, and the inlet and outlet pipes pass through the front panel of the inner container. At the same time, weld the filling port on the remaining two holes in the front panel of the inner container. The filling port is used to fill the paraffin phase change material into the inner container after the equipment is assembled, so the inner wall of the pipe needs to be cleaned after welding to prevent contamination and filling of phase change material.

Inner tank size control

XPS insulation layer shall be installed outside the inner container after welding. In order to ensure the installation and insulation effect of the insulation layer, the size of the inner container after welding shall be strictly controlled.

4) Water pipe joint position and concentricity control

In order to ensure the assembly of radiator shell, inner container and XPS insulation layer, the position and concentricity of water pipe joint and fin pipe inlet and outlet are required to be extremely high.

Enclosure size control and strength assurance

Housing made of 304 stainless steel, 2mm thick. Welding does not require full welding, but welding must ensure structural strength. In the process of factory handling, sea transportation and air transportation, there should be no deformation and damage. The welding quantity is required to control the welding deformation while ensuring the strength of the shell to prevent assembly interference.

Solving measures for 2. welding process difficulties are as follows

1) Inner tank sealing control measures

Make welding test pieces according to weld joints and verify welding parameters of various joints

Make the welding operation instruction, specify the size of each weld and the corresponding WPS.

Leak detection after welding by water immersion and pressure retention

2) Cleaning measures after pipe welding

The dual pipeline system of fin tube inlet and outlet and filling port is simultaneously inflated and polished.

3) Inner tank size control measures

Finned tube uniform forging welding to reduce heat input, strict control of finned tube diagonal size

The inner container splicing parts are added with bayonet buckles. The buckles are spot welded and positioned before the box body is fully welded. After the measured dimensions meet the tolerance requirements, the sections are cross-staggered and fully welded.

4) Control measures for position and concentricity of water pipe joint

After accurate measurement by the vernier caliper, the pipe joint shall be fixed by four-point spot welding.

Detecting tube position and concentricity with special gauge

After passing the inspection, the four sections around the pipe shall be welded in cross dislocation.

Housing size control and strength assurance

Clarify the welding method of each joint of the base plate and perform welding WPS

Clarify the welding method of each joint of cover plate and perform welding WPS