Beijing Zhichong C7 Charging Cabinet Welding

1. The difficulties in the welding process are as follows:

Appearance surface flatness control

The frame back plate and side door shutter area must be fully welded to ensure sealing. At the same time, the flatness of the exterior surface is required to be controlled within 2.5mm, and the flatness of the non-shutter area is required to be controlled within 1.5mm.

In order to ensure the installation of the electronic display screen, the flatness of the display screen installation area is controlled within 1.0mm. In order to ensure the smooth installation of the decorative panel and the front door panel, the flatness shall be controlled within 2mm.

Adaptability of frame dimensions to door panel assembly

The appearance requirements of the main weld of the box body are extremely high. At the same time, due to the requirements of output and efficiency, full-automatic mechanized welding is adopted. The box body is spliced by L-shaped and U-shaped bending parts. The weld is a lap weld with a lap size of 0.6-0.8mm and a small weld bead size. In order to achieve high efficiency and high quality automatic welding, the welding machine stability, mechanical arm accuracy, welding speed wire feeding speed and welding parameters need to be accurately adjusted.

Cabinet inner chamber sealing control

A large number of electronic components are installed inside the cabinet, and the use environment is outdoor. In order to ensure the normal use of the equipment under various weather conditions, it is necessary to ensure the sealing inside the cabinet. At the same time, because the cabinet body is a multi-warehouse structure, and the number of parts is large, the parts are spliced with each other, and because of the demand for ventilation and heat dissipation, multiple shutter parts are configured, resulting in a great increase in the difficulty of ensuring the sealing of the cabinet body.

2. The following are the measures to address the difficulties in the welding process.

1) Control measures for the flatness of the exterior surface of the cabinet body

Make a special welding water tank, place the door panel in the water tank, and spread soaked felt cloth before welding to accelerate heat dissipation.

Make special welding tooling for the front door, press the welding process, control the flatness of the display screen installation area, and shape after welding.

Shutter welding seam laser welding segment dislocation cross welding, welding process synchronous water cooling cooling to accelerate heat dissipation control deformation. The shutter blade and the honeycomb hole of the door panel shall be roll-welded and then spot-welded for reinforcement.

Backplate stiffeners are laser welded and welded in segments. All parts shall be pressed and fixed during welding.

During the welding process of the door panel, the process support is used for pressing, and the flatness is controlled by post-welding shaping.

2) Assurance measures for the suitability of frame size and door panel assembly

Single-piece laser welding of the common column reduces the welding heat input, and the straightness is controlled within 1mm after welding.

The diagonal of the frame shall be measured for several times, and the diagonal shall be measured and appropriately reshaped after spot welding and full welding.

After welding the internal support of the frame, remeasure the diagonal again and shape it.

3) Tightness control measures for cabinet inner chamber

Make a special leak detection system. Leak detection of cabinet body can be transferred to the next process after passing through

According to the side leakage of small batch cabinet, the leakage point shall be defined, and the leakage area shall be fully welded.

According to the side leakage of small batch cabinet, the welding sealant area shall be clearly applied.